| Profil č. | Am/V (m-1) | Obvod (m2/bm) | Šířka pásnice (mm) |
|
|---|---|---|---|---|
| ze 3 stran | ze 4 stran | |||
| 100 | 200 | 218 | 0,567 | 100 |
| 120 | 182 | 202 | 0,686 | 120 |
| 140 | 167 | 187 | 0,805 | 140 |
| 160 | 154 | 169 | 0,918 | 160 |
| 180 | 143 | 159 | 1,040 | 180 |
| 200 | 133 | 147 | 1,150 | 200 |
| 220 | 125 | 140 | 1,270 | 220 |
| 240 | 118 | 130 | 1,380 | 240 |
| 260 | 114 | 127 | 1,500 | 260 |
| 280 | 111 | 124 | 1,620 | 280 |
| 300 | 105 | 116 | 1,730 | 300 |
| 320 | 98 | 110 | 1,770 | 300 |
| 340 | 93 | 106 | 1,810 | 300 |
| 360 | 89 | 102 | 1,850 | 300 |
| 400 | 83 | 97 | 1,930 | 300 |
| 450 | 79 | 93 | 2,030 | 300 |
| 500 | 76 | 89 | 2,120 | 300 |
| 550 | 76 | 87 | 2,220 | 300 |
| 600 | 75 | 86 | 2,320 | 300 |
| 650 | 74 | 85 | 2,420 | 300 |
| 700 | 73 | 82 | 2,52 | 300 |
| 800 | 72 | 81 | 2,71 | 300 |
| 900 | 70 | 78 | 2,91 | 300 |
| 1000 | 70 | 78 | 3,11 | 300 |
Sídlo společnosti:
J Seidl a spol., s.r.o. Husova 120,
544 01 Dvůr Králové nad Labem,
tel: 499 320 459, fax: 499 320 219
Technická kancelář:
Pražská 16, 102 21 Praha 10,
tel/fax: 281 017 369, mobil: 608 075 005,
e-mail: bohuslav@seidl.cz, web: www.seidl.cz
VOR-KOS v Hradci Králové, oddíl C, vložka 4,
bankovní spojení KB Trutnov 13443/601/0100
IČ: 00484016
© J. Seidl & spol., s.r.o. 2009
Realizace www stránek: Saturn-Toya