| Profil č. | Am/V (m-1) | Obvod (m2/bm) | Šířka pásnice (mm) |
|
|---|---|---|---|---|
| ze 3 stran | ze 4 stran | |||
| 100 | 250 | 265 | 0,561 | 100 |
| 120 | 250 | 264 | 0,677 | 120 |
| 140 | 235 | 253 | 0,794 | 140 |
| 160 | 222 | 234 | 0,906 | 160 |
| 180 | 211 | 225 | 1,020 | 180 |
| 200 | 200 | 212 | 1,140 | 200 |
| 220 | 182 | 196 | 1,260 | 220 |
| 240 | 167 | 178 | 1,370 | 240 |
| 260 | 160 | 171 | 1,480 | 260 |
| 280 | 154 | 164 | 1,600 | 280 |
| 300 | 143 | 152 | 1,720 | 300 |
| 320 | 129 | 142 | 1,760 | 300 |
| 340 | 121 | 135 | 1,790 | 300 |
| 360 | 114 | 128 | 1,830 | 300 |
| 400 | 105 | 120 | 2,110 | 300 |
| 450 | 96 | 113 | 2,210 | 300 |
| 500 | 91 | 107 | 1,910 | 300 |
| 550 | 90 | 104 | 2,010 | 300 |
| 600 | 89 | 102 | 2,310 | 300 |
| 650 | 87 | 100 | 2,410 | 300 |
| 700 | 85 | 96 | 2,5 | 300 |
| 800 | 84 | 94 | 2,7 | 300 |
| 900 | 81 | 90 | 2,9 | 300 |
| 1000 | 81 | 89 | 3,1 | 300 |
Sídlo společnosti:
J Seidl a spol., s.r.o. Husova 120,
544 01 Dvůr Králové nad Labem,
tel: 499 320 459, fax: 499 320 219
Technická kancelář:
Pražská 16, 102 21 Praha 10,
tel/fax: 281 017 369, mobil: 608 075 005,
e-mail: bohuslav@seidl.cz, web: www.seidl.cz
VOR-KOS v Hradci Králové, oddíl C, vložka 4,
bankovní spojení KB Trutnov 13443/601/0100
IČ: 00484016
© J. Seidl & spol., s.r.o. 2009
Realizace www stránek: Saturn-Toya