| Profil č. | Am/V (m-1) | Obvod (m2/bm) | Šířka pásnice (mm) |
|
|---|---|---|---|---|
| ze 3 stran | ze 4 stran | |||
| 80 | 372 | 429 | 0,328 | 46 |
| 100 | 334 | 388 | 0,400 | 55 |
| B0 | 315 | 360 | 0,475 | 64 |
| 140 | 291 | 336 | 0,551 | 73 |
| 160 | 269 | 310 | 0,623 | 82 |
| 180 | 255 | 292 | 0,698 | 91 |
| 200 | 234 | 269 | 0,768 | 100 |
| 220 | 221 | 254 | 0,848 | 110 |
| 240 | 205 | 236 | 0,922 | 120 |
| 270 | 197 | 227 | 1,040 | 135 |
| 300 | 188 | 215 | 1,160 | 150 |
| 330 | 175 | 200 | 1,250 | 160 |
| 360 | 163 | 186 | 1,350 | 170 |
| 400 | 152 | 173 | 1,470 | 180 |
| 450 | 143 | 162 | 1,610 | 190 |
| 500 | 133 | 150 | 1,74 | 200 |
| 550 | 124 | 140 | 1,880 | 210 |
| 600 | 115 | 129 | 2,001 | 220 |
Sídlo společnosti:
J Seidl a spol., s.r.o. Husova 120,
544 01 Dvůr Králové nad Labem,
tel: 499 320 459, fax: 499 320 219
Technická kancelář:
Pražská 16, 102 21 Praha 10,
tel/fax: 281 017 369, mobil: 608 075 005,
e-mail: bohuslav@seidl.cz, web: www.seidl.cz
VOR-KOS v Hradci Králové, oddíl C, vložka 4,
bankovní spojení KB Trutnov 13443/601/0100
IČ: 00484016
© J. Seidl & spol., s.r.o. 2009
Realizace www stránek: Saturn-Toya