| The set of catalogue sheets Valid from 15.07.2004 Version ČSN EN 13501-2 |
EI 15 - 120 |
03 | 03303 |
Caution: these pages serve only for the first information about material for designers and investors, they are solved in one uniform chart and they don't pose pretentions on perfections. Other basis or details can be found out in our technical office. Data written in this list agree with by this time publicated data and obtained experience of J.SEIDL a spol.., s.r.o. Supplier is not in charge of applications done out of frame here given tests and certifications - operations of fire fighting applications with product mentioned in this list without written authorisation of producer or author are prohibited.
Product Catalogue Sheet
System of glued facings for steel constructions serving as fire-separating constructions (ridges) in places with poor heat outlet from exposed and non-exposed side. Facings are made of the slabs that are on mineral felt base, guyed by fireproof mastic sealant and metal couplers. The basis is ORSIL PYRO slabs made by molten mass pulping from mixture of basalt, blast-furnace slag and diabase and furthermore fireproof dispersing adhesive. The slabs do not contain any asbestos fibres.
Appearance: The facings are without any additional surface finishing from light brown colour to grey-green colour with geometric screen on the surface. Commissures and joints are agglutinated with different coloured mastic. The slab surface is without any additional coating porous and coarse.
Surface finishing: In virtue of customer special demand, the final facing surface can be unified in colour with a special stone paint, provided in basic white colour. Plastering reinforced with glass fibre net can alternatively cover the surface.
The system is designed for steel technological and non-bearing constructions outer side of storage containers, tanks and chemical apparatus and equipment from EI 15 to EI 120 minutes.
Facings are suitable for:Industrial environment with industrial atmosphere to 4th degree and for all ordinarily heated and heatless interiors. Facings constantly lag protected structure (heat leaks), they can even substitute additional heat insulation of the same thickness. Bearing elements do not bear, crackle and they tolerate even shakes and dynamic shocks of protected structure. Surface-finished facing can be exposed outdoors in case there are not extremely aggressive conditions.
Facings are not suitable for:Facings must not be exposed to dripping or flowing water without any additional surface finishing. Maximum permissible permanent relative air humidity is 85%.
Supply and fix is provided exclusively by J. SEIDL & spol.s r.o. company where is possible to apply all your requirements, eventually companies that own the written licence from J. SEIDL & spol.s r.o. company for using the industrial rights for this solution.
When facings are used according to point B and when all specified technological procedures are kept, facings fulfil the regulations of § 47 s. 1, Building Act.
Firefighting glued facings ORDEXAL were examined by accredited testing station PAVÚS - Veselí n. L. and certificated by this organization. On the basis of above mentioned examinations and expert opinions, this organization made the following table, showing the values of welding panel fire resistance increasing and apparatuses fire resistance increasing with different facings thickness in case when the fire effects the side with facing and in case that the fire effects the unprotected side.
| Fire resistance | ORDEXAL slab thickness (mm) | |||||
| Fire from side with ORDEXAL facing | Fire effects on the metal plate | |||||
| Metal plate thickness in mm | Metal plate thickness in mm | |||||
| 3 | 6 | 10 | 3 | 6 | 10 | |
| EI 15 | 20 | 20 | 20 | 40 | 40 | 40 |
| EI 30 | 40 | 40 | 20 | 60 | 60 | 60 |
| EI 45 | 60 | 60 | 40 | 80 | 80 | 80 |
| EI 60 | 80 | 60 | 60 | 100 | 100 | 400 |
| EI 90 | 100 | 80 | 80 | 120 | 120 | 120 |
| EI 120 | 120 | 100 | 100 | 140 | 140 | 140 |
The application of ORDEXAL system is tied by set know-how and by strict material structure in accordance with examined samples (in PAVÚS Veselí n. L) and with valid expert opinions. Because of this reason, the application can be provided only by companies trained by J. SEIDL & spol. (that is the only owner of all industrial rights for this application) and by companies that own the written authorizationThe certificate, The Declaration of Conformity or any other documents do not refer to completed work without this written authorization.
During the application it is necessary to use the protective aids, i.e. leather gloves, safety glasses or shield, respirator when shaping or cutting, if there is a need, protective apron and after work ending and before every meal - to wash hands with water and use the barrier cream.
ČSN series 73 08.., ČSN EN 1363-1, ČSN P ENV 1995-1-2, ČSN EN 13501-2 and set of experts' reports PAVÚS a.s., certificates, technical data and other documentation and producers' materials and materials of J. SEIDL & spol. s r.o. company.
J.Seidl & spol.,s.r.o. Technical office, Pražská 16, 102 21 Praha 10 - Hostivař, tel./fax: 281017363, E-mail: seidl@comp.cz; E. Vašátko, expert in "Materials in firefighting protection".
Sídlo společnosti:
J Seidl a spol., s.r.o. Husova 120,
544 01 Dvůr Králové nad Labem,
tel: 499 320 459, fax: 499 320 219
Technická kancelář:
Pražská 16, 102 21 Praha 10,
tel/fax: 281 017 369, mobil: 608 075 005,
e-mail: bohuslav@seidl.cz, web: www.seidl.cz
VOR-KOS v Hradci Králové, oddíl C, vložka 4,
bankovní spojení KB Trutnov 13443/601/0100
IČ: 00484016
© J. Seidl & spol., s.r.o. 2009
Realizace www stránek: Saturn-Toya